Inspection of the roof revealed unexpected levels of decay. 30% of the
roof decking and 5% of the rafters required replacement or reinforcement.
Epoxy treatment was utilized wherever possible to allow for a larger
percentage of the original roof to remain intact. Insulation and an
ice and water shield were installed to make the repaired roof watertight.  |